T.P. Gabb, J. Telesman, and L. Ghosn Glenn Research Center, Cleveland, Ohio A. Garg University of Toledo, Toledo, Ohio J. Gayda Glenn Research Center, Cleveland, Ohio Factors Influencing Dwell Fatigue Cracking in Notches of Powder Metallurgy Superalloys NASA/TM—2011-217118 June 2011