Transgranular Stress Corrosion Cracking MUHAMMAD ARIF SAADILAH 1406507285
Transgranular Stress
Corrosion CrackingMUHAMMAD ARIF SAADILAH
1406507285
Layout
Definition
Characteristics
Factors
Corrosion
Crack
Mechanism
Study Case 1
Definition
Factors Specific Crystal Planes
Low Indices: [100], [110], [210]
Speciffic Electrochemical
Cracking Mechanism
Characteristics of SCC
Corrosion type: Pitting
Prevention
Lowering the stress
Eliminating the critical environmental species
Adding Inhibitors
Coatings
Changing the material
Shot-peening / Shot Blasting
Applying cathodic protection
Study Case
Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineriesAlmubarak and M. Belkharchouche & A. Husain
Anti-Corrosion Methods and Materials
Volume 57 · Number 2 · 2010 · 58–64
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries – Introduction -
Austenite
- H2S
- Sour Gas
- Polythionic Acid
Kuwait
Petroleum Reinaries
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries
– Materials-
• Annealed by 1080 C, thn
water quenching
• Sensitizing heat 650 C then
air cooling
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries – Methods-
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait petroleum refineries
– Results-
• Sensitized austenitic stainless steel type 304 in polythionic acid
• sensitized austenitic stainless steel type 304 in sour
solution
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries – Results-
sensitized austenitic stainless steel type 304 in chloride solution
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries – Results-
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries – Results-
a) Sensitized austenitic stainless steel type 321 in polythionic acid;
b) sensitized austenitic stainless steel type 321 in sour solution;
c) sensitized austenitic stainless steel type 321 in chloride solution;
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries – Results-
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries – Result-
the polythionic acid is the primary contributory agent for cracking
Types 304 and 316 stainless steel are unsuitable for longterm
exposure in sulfide service above 4008C because of sensitization.
sensitization evidently accelerates SCC and causes cracking to
occur easily
The present investigation was done in a short period (45 days)
for different grades of sensitized stainless steel where cracking and
severe SCC occurred.
Case Study: Stress corrosion cracking of sensitized
austenitic stainless steels in Kuwait
petroleum refineries – Conclusion-
Terima Kasih