University of Nebraska - Lincoln DigitalCommons@University of Nebraska - Lincoln Civil Engineering Faculty Publications Civil Engineering 5-2014 Nanoindentation Test Integrated with Numerical Simulation to Characterize Mechanical Properties of Rock Materials Hoki Ban Hanyang University, [email protected] Pravat Karki University of Nebraska - Lincoln, [email protected] Yong-Rak Kim University of Nebraska - Lincoln, [email protected] Follow this and additional works at: hps://digitalcommons.unl.edu/civilengfacpub is Article is brought to you for free and open access by the Civil Engineering at DigitalCommons@University of Nebraska - Lincoln. It has been accepted for inclusion in Civil Engineering Faculty Publications by an authorized administrator of DigitalCommons@University of Nebraska - Lincoln. Ban, Hoki; Karki, Pravat; and Kim, Yong-Rak, "Nanoindentation Test Integrated with Numerical Simulation to Characterize Mechanical Properties of Rock Materials" (2014). Civil Engineering Faculty Publications. 84. hps://digitalcommons.unl.edu/civilengfacpub/84