10/27/14 Keysight G200 Nanoindenter (formerly Agilent) Location White Bldg. Room 613
10/27/14
Keysight G200 Nanoindenter (formerly Agilent)
Location White Bldg. Room 613
10/27/14 Keysight Nanoindenter (formerly Agilent)
10/27/14 Keysight Nanoindenter
Capabilities: • Determining Modulus at specified depth. •Using Continuous Stiffness Module to determine Modulus as a function of depth (CSM). •Determining modulus and hardness though the thickness of coatings.
10/27/14 Keysight Nanoindenter
Sample Tray
(4) Samples can be loaded at one time.
Sample size limitation 30 mm diameter x 25-28 mm tall cylinder
10/27/14 Keysight Nanoindenter
Quick access to samples without exchange of entire environment.
10/27/14 Keysight Nanoindenter
Data / Results are displayed and exported easily to Excel.
-50
0
50
100
150
200
250
300
-200 0 200 400 600 800 1000 1200 1400 1600
mN
nm
Loading / Unloading on Calibration Standard – Fused Silica
10/27/14 Nanoindenter Example Output
10/27/14
More information can be located @ Keysight’s website:
10/27/14
Thank you