Corner welds on test cubes Erno Roeland, Tjeerd Ketel 17-03-2011 1 Nikhef VertxMT
Feb 15, 2016
Nikhef VertxMT 1
Corner welds on test cubes
Erno Roeland, Tjeerd Ketel
17-03-2011
Nikhef VertxMT 2
The test cubes
1 2 3 4
5 6
17-03-2011
Nikhef VertxMT 3
Cubes 1-4
• Cube 1:– Test of flat foils, without good cooling contact.
• Cube 2:– 12A. All corners bad. Both solder and weld added
• Cube 3:– 17A. All corners bad. Little cracks. Repairs failed.
• Cube 4:– 19A. Three corners bad. Weld added. One repaired
17-03-2011
Nikhef VertxMT 4
Plans
• Finish cubes 4 and 5.• Start welding two real boxes.• (Start corner tests in flange.)
17-03-2011