Washington University in St. Louis Washington University in St. Louis Washington University Open Scholarship Washington University Open Scholarship McKelvey School of Engineering Theses & Dissertations McKelvey School of Engineering Spring 5-15-2017 Characterizing Structure, Properties, and Deformation in Metallic Characterizing Structure, Properties, and Deformation in Metallic Glasses and Olivine Using Instrumented Nanoindentation Glasses and Olivine Using Instrumented Nanoindentation Kelly Kranjc Washington University in St. Louis Follow this and additional works at: https://openscholarship.wustl.edu/eng_etds Part of the Materials Science and Engineering Commons, and the Mechanics of Materials Commons Recommended Citation Recommended Citation Kranjc, Kelly, "Characterizing Structure, Properties, and Deformation in Metallic Glasses and Olivine Using Instrumented Nanoindentation" (2017). McKelvey School of Engineering Theses & Dissertations. 241. https://openscholarship.wustl.edu/eng_etds/241 This Dissertation is brought to you for free and open access by the McKelvey School of Engineering at Washington University Open Scholarship. It has been accepted for inclusion in McKelvey School of Engineering Theses & Dissertations by an authorized administrator of Washington University Open Scholarship. For more information, please contact [email protected].