Radiographic Interpreter: Weld Defect Exercise Part 1
Post on 23-Jun-2015
932 Views
Preview:
DESCRIPTION
Transcript
ASNT RT LEVEL 2
IN-HOUSE TRAINING
AL-USWAH INSPEKSITAMA
NDT TRAINING CENTER
Jl. Raya Natar No. 55, Pasar Lama Natar Lampung Selatan
Telp. 0721-91025 / 081369255454 E-mail: al.uswah.ndt@gmail.com
X1
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X2
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X3
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X4
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X5
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X6
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X7
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X8
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X9
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
X10
AL-USWAH INSPEKSITAMA NDT TRAINING CENTER
JAWABAN
� X1 No Defect
� X2 Elongated Cavity
� X3 Distributed Porosity
� X4 Clustered Porosity
� X5 Linear Porosity
� X6 Linear Slag Inclusion
� X7 Continuous Undercut
� X8 Incomplete Penetration
� X9 Worm Hole
� X10 Root Fusion